    • Abstract

       

      We report the density depth profile of an as-deposited Ni film and density profile for the same film after controlled electrochemical corrosion by chloride ions, measured by unpolarized neutron reflectometry. The neutron reflectometry measurement of the film after corrosion shows density degradation along the thickness of the film. The density profile as a function of depth, maps the growth of pitting and void networks due to corrosion. The profile after corrosion shows an interesting peaking nature.

    • Author Affiliations

       

      Surendra Singh1 A K Poswal2 S K Ghosh3 Saibal Basu1

      1. Solid State Physics Division; Bhabha Atomic Research Centre, Mumbai 400 085, India
      2. Spectroscopy Division; Bhabha Atomic Research Centre, Mumbai 400 085, India
      3. Material Processing Division, Bhabha Atomic Research Centre, Mumbai 400 085, India
    • Dates

       
  • Pramana – Journal of Physics | News

    • Editorial Note on Continuous Article Publication

      Posted on July 25, 2019

      Click here for Editorial Note on CAP Mode

© 2017-2019 Indian Academy of Sciences, Bengaluru.