      Electrical conductivity; thermoelectric power; dielectric constant; copper tungstate

    • Abstract

       

      The temperature dependence of the electrical conductivity, thermoelectric power and dielectric constant of the antiferromagnetic CuWO4 have been studied in the temperature range 300–1000 K. The conductivity results can be summarised by the equations σI=6.31 × 10−3 exp (−0.29 eV/kT) ohm−1 cm−1 in the temperature range 300–600 K and σII=3.16 × 105 exp (−1.48 eV/kT) ohm−1 cm−1 between 600 K and 1000 K. The thermoelectric power can be expressed byθ=[− 1.25 (103/T) + 3.9] mV/K. Initially dielectric constant increases slowly but for high temperatures its increase is fast.

    • Author Affiliations

       

      R Bharati1 R Shanker1 R A Singh1

      1. Department of Physics, University of Gorakhpur, Gorakhpur - 273 001, India
    • Dates

       
  • Pramana – Journal of Physics | News

    • Editorial Note on Continuous Article Publication

      Posted on July 25, 2019

      Click here for Editorial Note on CAP Mode

© 2017-2019 Indian Academy of Sciences, Bengaluru.