On critical hydrogen concentration for hydrogen embrittlement of Fe3Al
A Priyadarshi R Balasubramaniam
Click here to view fulltext PDF
Permanent link:
https://www.ias.ac.in/article/fulltext/boms/024/05/0559-0562
The critical hydrogen concentration for hydrogen embrittlement in iron aluminide, Fe3Al has been estimated (0.42 wppm). The estimated critical hydrogen content has been correlated to structural aspects of the decohesion mechanism of hydrogen embrittlement.