      Microstructure; grain size

    • Abstract

       

      XRD and microstructure studies were carried out on Ti4+ and Zr4+-substituted Li-Zn ferrites prepared by standard ceramic technique. All the ferrite compositions exhibit single phase formation. The lattice parametera increases linearly with the content of Zn2+Zr4+ and Zn2+Ti4+, which is attributed to the ionic volumes of the cations involved. With substitution by Zr4+ the average size decreases, while with substitution by Ti4+ the grain size increases. In both the series grain size varies with the composition. Excess substitution of Zr4+ (x>0·4) leads to the formation of secondary images and discontinuous grain growth. Both Zr4+ and Ti4+ compositions obey Kurtz theory.

    • Author Affiliations

       

      R S Patil1 S S Suryavanshi1 2 S V Kakatkar1 A M Sankpal1 U R Ghodake1 2 S A Patil1 S R Sawant1

      1. Department of Physics, Shivaji University, Kolhapur - 416 004, India
      2. Department of Physics, Shivaji University, Centre for Post-Graduate Studies, Solapur - 413 003, India
    • Dates

       
  • Bulletin of Materials Science | News

    • Dr Shanti Swarup Bhatnagar for Science and Technology

      Posted on October 12, 2020

      Prof. Subi Jacob George — Jawaharlal Nehru Centre for Advanced Scientific Research, Jakkur, Bengaluru
      Chemical Sciences 2020

      Prof. Surajit Dhara — School of Physics, University of Hyderabad, Hyderabad
      Physical Sciences 2020

    • Editorial Note on Continuous Article Publication

      Posted on July 25, 2019

      Click here for Editorial Note on CAP Mode

© 2021-2022 Indian Academy of Sciences, Bengaluru.